Edge or shoulder cracking can be identified by its location on the pavement; the cracks run longitudinally, located within one or two feet of the edge of the asphalt. This is caused by poor drainage, a lack of support at the asphalt edge, the structural support compromised by heavy vegetation and/or heavy traffic along the edge, or underlying layers weakened due to settlement of underlying material or shrinkage of drying out soil.
GAP Mastic is a hot-applied material designed for situations where crack sealants are ineffective or insufficient and where repaving is impractical or cost-prohibitive. GAP Mastic combines the flexibility and adhesion of rubberized asphalt sealants with the strength and load-bearing qualities of engineered aggregates. Featuring InteliBondTM active bonding technology and our revolutionary PolySkinTM meltable packaging, GAP Mastic provides a stable, flexible repair that bonds firmly with the existing pavement edge/shoulder to seal out water and debris and protect against further damage.